Implantable biocompatible reactor
Réacteur implantable biocompatible
Résumé
The invention concerns a bioreactor obtained by compressing a mixture of an enzyme, a conductor and chitosan. The conductor can consist of carbon nanotubes. This bioreactor can be produced according to the following steps: preparing a mixture of powders in which the proportion of enzyme powder relative to a carbon nanotube powder is of the order of 50/50 by weight; preparing a viscous solution of chitosan in a ratio of 5 to 15 (in mg) of chitosan to 0.75 to 1.25 (in ml) of acetic acid diluted to 0.4 to 0.6% by volume in water; adding the viscous chitosan to the mixture of powders in a proportion be weight of 3 to 5 of powder to 5 to 10 of chitosan; carrying out a first compression followed by light grinding; carrying out a second compression to produce a pellet; and drying at ambient temperature.
L'invention concerne un bioréacteur obtenu par compression d'un mélange d'une enzyme, d'un conducteur et de chitosane. Le conducteur peut être constitué de nanotubes de carbone. Ce bioréacteur peut être fabriqué selon les étapes suivantes : préparer un mélange de poudres dans laquelle la proportion de poudre d' enzyme par rapport à une poudre de nanotubes de carbone est de l'ordre de 50/50 en poids ; préparer une solution visqueuse de chitosane dans un rapport de 5 à 15 (en mg) de chitosane à 0,75 à 1,25 (en ml) d'acide acétique dilué à 0,4 à 0,6 % en volume dans de l'eau ; ajouter au mélange de poudres la chitosane visqueuse dans une proportion pondérale de 3 à 5 pour la poudre à 5 à 10 pour la chitosane ; procéder à une première compression puis à un broyage léger ; procéder à une deuxième compression pour réaliser une pastille ; et sécher à température ambiante.